Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Sinelec CCB1834 Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Teknor Apex Company
Trade Name Sinelec
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Sinelec CCB1834 Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Electrically Conductive Forms: Pellets Processing Method: Injection MethodInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
ASTM D792
Melt Flow 1.40 g/10 min

@Load 5.00 kg,
Temperature 230 °C
1.40 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
5.60 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.60 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638
Flexural Strength 28.0 MPa
4060 psi
ASTM D790
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Izod Impact, Notched 2.99 J/cm

@Temperature 22.8 °C
5.60 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 97.8 °C
208 °F
Unannealed; ASTM D648
Vicat Softening Point 151 °C
304 °F
Loading 1 (10N); ASTM D1525
Electrical Properties Metric English Comments
Volume Resistivity 1e+05
1e+05
ASTM D257
Surface Resistance 1e+05
1e+05
ASTM D257
Copyright © lookpolymers.com All Rights Reserved