Teknor Apex Sinpolene MBB1401 Linear Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Compounding Resin
Manufacturer Teknor Apex Company
Trade Name Sinpolene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Sinpolene MBB1401 Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (480000 ppm) Features: Recyclable Material Uses: Compounding Forms: Pellets Processing Method: Injection Method; Compounding Additional Information: Recommended Dosage: 2.0-5.0%Information Provided by Teknor Apex
Physical Properties Metric English Comments
Melt Flow 70.0 g/10 min

@Load 10.0 kg,
Temperature 190 °C
70.0 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ASTM D1238
Descriptive Properties Value Comments
Appearance Black