Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Sinvicomp SIH 5005 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name Sinvicomp
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Sinvicomp SIH 5005 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: Asia Pacific Features: High Heat Resistance; Good Stiffness Uses: Electronic Insulation; Wire and Cable Applications Wire Types: Class 1/1; Type 4; Type 5 Agency Ratings: BS 6746; UL 1581; JIS 6723 Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 93
93
ASTM D2240
Tensile Strength, Yield 17.62 MPa
2556 psi
Change in tensile strength after 240 hours at 275°F; ASTM D638
19.6 MPa
2840 psi
9.8 in/min; ASTM D638
Elongation at Break 212.5 %
212.5 %
Change after 240 hours at 275°F; ASTM D638
250 %
250 %
9.8 in/min; ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 190 °C

@Time >=7200 sec
374 °F

@Time >=2.00 hour
Congo Red; BS 2782