Material Notes:
Availability: Asia Pacific Features: Medium Impact Resistance Uses: Electrical/Electronic Applications Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Melt Flow 17.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
17.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 57.8 MPa
8390 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Izod Impact, Notched 0.390 J/cm
0.730 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 190 °C

@Time 1800 sec
374 °F

@Time 0.500 hour
Congo Red; BS 2782
Vicat Softening Point 86.1 °C
187 °F
ASTM D1525