Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
15 Seconds
80
80
ASTM D2240
Tensile Strength, Yield 7.58 MPa
1100 psi
ASTM D412
Elongation at Break 690 %
690 %
ASTM D412
100% Modulus 0.00228 GPa
0.330 ksi
ASTM D412
300% Modulus 0.00331 GPa
0.480 ksi
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746