Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00228 GPa | 0.330 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR Laminar Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00228 GPa | 0.330 ksi | ASTM D412 |
Teknor Apex TELCAR® 1050-75 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
100% Modulus | 0.00228 GPa | 0.330 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR Laminar Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |