Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Terraloy™ BP 13000A Thermoplastic Starch + PP

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Teknor Apex Company
Trade Name Terraloy™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Terraloy™ BP 13000A Thermoplastic Starch + PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: Terraloy™ BP-13000A is a Thermoplastic Starch/PP ready-to-process compound that contains up to 30% of TPS renewable content. This compound is intended for injection molding as well as extrusion applications. Processing Method: Extrusion; Injection Molding Forms: Pellets Additional Information: Biobased Content: < 30.0Information Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.997 g/cc
0.997 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 21.0 MPa
3040 psi
ASTM D638
Elongation at Break 75 %
75 %
ASTM D638
Tensile Modulus 1.12 GPa
163 ksi
ASTM D638
Flexural Strength 32.5 MPa

@Strain 5.00 %
4720 psi

@Strain 5.00 %
ASTM D790B
Flexural Modulus, 1% Secant 1060 MPa
154000 psi
ASTM D790B
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
ASTM D256
Izod Impact, Unnotched 11.7 J/cm
22.0 ft-lb/in
ASTM D4812