Teknor Apex UNIPRENE® 7100-50D Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Teknor Apex Company
Trade Name UNIPRENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex UNIPRENE® 7100-50D Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 48
48
10 seconds; ASTM D2240
55
55
10 seconds; ASTM D2240
Tensile Strength, Yield 22.8 MPa
3300 psi
ASTM D412
Elongation at Break 600 %
600 %
ASTM D412
100% Modulus 0.0145 GPa
2.10 ksi
ASTM D412
Tear Strength 114 kN/m
650 pli
ASTM D624
Compression Set 44 %
44 %
23°C, 22 hr.; ASTM D395, Method B
80 %
80 %
100°C, 22 hr.; ASTM D395, Method B
Thermal Properties Metric English Comments
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746