Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ter Hell Plastic Terez® PA 6 7450 T GK 30 Polyamide 6, 30% Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Bead Filled
Manufacturer Ter Hell Plastic GMBH
Trade Name Terez®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ter Hell Plastic Terez® PA 6 7450 T GK 30 Polyamide 6, 30% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamide 6 medium viscosity, heat impact resistant and 30% glass bead reinforced.Application: For low warpage molding parts with balanced shrinkage characteristics.Information provided by Ter Hell Plastic GMBH.
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ISO 1183
Water Absorption 5.7 %
5.7 %
ISO 62
Moisture Absorption at Equilibrium 1.8 %
1.8 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength 55.0 MPa
7980 psi
dry; ISO 527
Tensile Strength, Yield 60.0 MPa
8700 psi
dry; ISO 527
Elongation at Break 20 %
20 %
dry; ISO 527
Tensile Modulus 2.90 GPa
421 ksi
dry; ISO 527
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
dry; ISO 179
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
dry; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 175 °C
347 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ISO 75
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Processing Properties Metric English Comments
Processing Temperature 240 - 270 °C
464 - 518 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour