Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® C6850REC PC+ABS (Europe-Africa-Middle East) PC+ABS Industrial quality. Flame retardant. Limited colors only (Black and Grey)This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycoloy® CY5220 PC+ABS (Asia Pacific) Non-chlorinated & non-brominated FR PC/ABS featuring good flow and impact properties. Designed for various thin wall applicationsThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Europe-Africa-Middle East) This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® DMX2415 PC (Europe-Africa-Middle East) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Europe.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Dry Blend E7364 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Faradex DS0026 PC (Europe-Africa-Middle East) LNP* Faradex* DS0026 is a compound based on Polycarbonate resin containing Flame Retardant, Stainless Steel Fiber. Added features include: EMI/RFI Shielding, Flame Retardant, Non-Brominated & Non-C.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | ASTM D638 |
LNP Lubricomp® LL-4040 Polyetheretherketone, PTFE Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | ASTM D638 |
Plaskolite Optix® PL-150 Acrylic Resin
(discontinued **) Injection/extrusion pellets.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Tensile Modulus | 2.90 GPa @Temperature 23.0 °C |
421 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 7331J NC010 Nylon 6
(Unverified Data**) Zytel® 7331J NC010 is lubricated fast cycling PA6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | |
Henkel Hysol EA 9321 Paste Adhesive System Thixotropic adhesive that yields tough, durable bonds over a wide temperature range.Applications: Potting Structural Repair |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | |
LATI Latigray 52/11-01 CX/70 PP Homopolymer Radiopaque compound based on Polypropylene homopolymer (PPh). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | DIN 53457 |
Schwartz Technical Plastics LAMIGAMID® 309 Cast Polyamide 6, Oil Filled, Dry Application: slippers, inserts for coupling boxes, wear linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem DH1004F PEI High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas regi.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM HU1004 PEI (Europe-Africa-Middle East) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM UF5011S PEI Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM UF5011S PEI (Asia Pacific) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® VX5005 PBT (Europe-Africa-Middle East) VALOX VX5005 is a 5% glass fibre reinforced, impact modified PBT+PC blend with low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | dry; ISO 527 |
Ter Hell Plastic Terez® PA 6 7450 T GK 30 Polyamide 6, 30% Glass Fiber Description: Polyamide 6 medium viscosity, heat impact resistant and 30% glass bead reinforced.Application: For low warpage molding parts with balanced shrinkage characteristics.Information provide.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 1mm/min; ISO 527-1, 2 |
Polyplastics TOPAS® 6013 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) Due to its high transparency, low levels of eluates, superior chemical resistance, and high heat deflection temperature, this grade is suitable for products such as pharmaceutical packaging and diag.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | ASTM-D790 |
Polyram RamSter RF350M3 PBT, 15% Mineral Filled 15% mineral filled PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BGZ-15 PA6-GF15 Information provided by EMS Grivory |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | ISO 527-1/-2 |
DSM Stanyl® TW371 (DAM) Nylon 46 Heat Stabilized, PTFE Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | ISO 527 - 1 & - 2 |
Asahi Kasei Tenac® SH210 Homopolymer Acetal Resin Super high-impact grade; highest molecular weight category.Information provided by Asahi Kasei Corporation. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | |
LATI Latigea B01 I6 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p... |