Material Notes:
Information provided by TERIO Corporation.
Physical Properties Metric English Comments
Particle Size 0.40 - 25 µm
0.40 - 25 µm
PSD (d<sub>50</sub>
Specific Surface Area 1.0 - 50 m²/g
1.0 - 50 m²/g
Component Elements Properties Metric English Comments
Y2O3 0.00 %
0.00 %
ZrO2 99.5 %
99.5 %