Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 1.0 - 50 m²/g | 1.0 - 50 m²/g | |
Terio Corporation TZ-1~30 Zirconia Information provided by TERIO Corporation. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Antimony Nanoparticles General DescriptionAntimony (Sb) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Antimony Particles are typically 20-40 nano.. |
|||
Specific Surface Area | 10 - 50 m²/g | 10 - 50 m²/g | |
American Elements Antimony Oxide Nanopowder General DescriptionAntimony Oxide ( SbO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. N.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Europium Nanoparticles General DescriptionEuropium (Eu) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Europium Particles are typically 10 - 45 nanometers (nm) with specif.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Gadolinium Nanoparticles General DescriptionGadolinium (Gd) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Gadolinium Particles are typically 10 - 45 nanometers (nm) with sp.. |
|||
Specific Surface Area | 25 - 50 m²/g | 25 - 50 m²/g | |
American Elements Hafnium Oxide Nanopowder General DescriptionHafnium Oxide or Hafnia Nanopowder or Nanoparticles (HfO), nanodots or nanocrystals are white high surface area particles. Nanoscale Hafnium Oxide Nanoparticles are typically 5 - .. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Indium Nanoparticles General DescriptionIndium (In) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Indium Particles are typically 20-40 nanomete.. |
|||
Specific Surface Area | 25 - 50 m²/g | 25 - 50 m²/g | |
American Elements Indium Oxide Nanopowder General DescriptionIndium Oxide Nanopowder or Nanoparticles (InO), nanodots or nanocrystals are white high surface area particles. Nanoscale Indium Oxide Nanoparticles are typically 5 - 100 nanomete.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Iron Cobalt Nanopowder General DescriptionIron Cobalt ( FeCo) Nanopowder or Nanoparticles, nanodots or nanocrystals are black spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Iron Nickel Nanopowder General DescriptionIron Nickel ( FeNi) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties. Nano.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Iron Oxide Nanopowder General DescriptionIron Oxide ( Fe2O3 and Fe3O4) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure part.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Lanthanum Nanoparticles General DescriptionLanthanum (La) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Lanthanum Particles are typically 5 - 40 nanometers (nm) with speci.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Lead Oxide Nanopowder General DescriptionLead Oxide ( PbO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Lead Oxide Par.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Lithium Manganese Dioxide Nanoparticles General DescriptionLithium Manganese Oxide (LiMnO) Nanoparticles, nanodots or nanopowder are spinel, high surface area particles. Nanoscale Lithium Manganese Oxide Particles are typically 10 - 50 na.. |
|||
Specific Surface Area | 5.0 - 50 m²/g | 5.0 - 50 m²/g | |
American Elements Lithium Vanadate Nanoparticles General DescriptionLithium Vanadate or Lithium Vanadium Oxide (LiVO) Nanoparticles, nanodots or nanopowder are spinel, high surface area particles. Nanoscale Lithium Vanadate or Lithium Vanadium Oxi.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Lutetium Nanoparticles General DescriptionLutetium (Lu) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Lutetium Particles are typically 10 - 100 nanometers (nm) with speci.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Manganese Nanoparticles General DescriptionManganese (Mn) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Manganese Particles are typically 20-40 na.. |
|||
Specific Surface Area | 25 - 50 m²/g | 25 - 50 m²/g | |
American Elements Manganese Oxide Nanopowder General DescriptionManganese Oxide Nanopowder (MnO), nanodots or nanoparticles are high surface area particles. Nanoscale Manganese Oxide Nanoparticles are typically 5 - 100 nanometers (nm) with spe.. |
|||
Specific Surface Area | 10 - 50 m²/g | 10 - 50 m²/g | |
American Elements Molybdenum Oxide Nanopowder General DescriptionMolybdenum Oxide ( MoO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles... |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Nickel Titanium Nanoparticles General DescriptionNickel Titanium (NiTi) Nanoparticles, nanodots or nanopowder are black spherical high surface area alloy particles. Nanoscale Nickel Titanium Particles are typically 10 - 40 nanom.. |
|||
Specific Surface Area | 25 - 50 m²/g | 25 - 50 m²/g | |
American Elements Niobium Oxide Nanoparticles General DescriptionNiobium Oxide ( MoO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Na.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Praseodymium Nanoparticles General DescriptionPraseodymium (Pr) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Praseodymium Particles are typically 10 - 45 nanometers (nm) wit.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Samarium Nanoparticles General DescriptionSamarium (Sm) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Samarium Particles are typically 10 - 50 nanometers (nm) with specif.. |
|||
Specific Surface Area | 25 - 50 m²/g | 25 - 50 m²/g | |
American Elements Silicon Oxide Nanopowder General DescriptionSilicon Oxide (SiO2) Nanopowder, Silica Nanoparticles or nanodots are high surface area particles. Nanoscale Silicon Oxide Nanoparticles or Silica Particles are typically 5 - 100 .. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Strontium Carbonate Nanoparticles General DescriptionStrontium Carbonate (SrCO3) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Strontium Carbonate Particles are typically 5 - 40 nan.. |
|||
Specific Surface Area | 25 - 50 m²/g | 25 - 50 m²/g | |
American Elements Yttria stabilized Zirconia General DescriptionYttria stabilized Zirconia or Zirconium Oxide Nanopowder or Nanoparticles (YSZ), nanodots or nanocrystals are white high surface area particles available fully stabilized (8 mol%).. |
|||
Specific Surface Area | 25 - 50 m²/g | 25 - 50 m²/g | |
American Elements Zirconium Oxide Nanopowder General DescriptionZirconium Oxide or Zirconia Nanopowder or Nanoparticles (ZrO2), nanodots or nanocrystals are white high surface area particles available in monoclinic or as stabilized or doped wi.. |
|||
Specific Surface Area | 15 - 50 m²/g | 15 - 50 m²/g | |
American Elements Calcium Oxide Nanopowder General DescriptionCalcium Oxide ( CaO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Na.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Carbon Nanoparticles General DescriptionCarbon (C) Nanoparticles, nanodots or nanopowder are black spherical high surface area graphitic carbon. Nanoscale Carbon Particles are typically 10 - 45 nanometers (nm) with spec.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Cobalt Iron Nanopowder General DescriptionCobalt Iron ( CoFe) Nanopowder or Nanoparticles, nanodots or nanocrystals are black spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties.. |