ThyssenKrupp 25CrMo4 Saw Steel, Hot-Rolled Strip

Category Metal , Ferrous Metal , Carbon Steel
Manufacturer ThyssenKrupp
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ThyssenKrupp 25CrMo4 Saw Steel, Hot-Rolled Strip.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat treatment: annealedSurface: pickled, pickled and oiledInformation Provided by Thyssen Krupp
Component Elements Properties Metric English Comments
Carbon, C 0.28 %
0.28 %
Chromium, Cr 1.0 %
1.0 %
Manganese, Mn 0.85 %
0.85 %
Molybdenum, Mo 0.20 %
0.20 %
Silicon, Si 0.20 %
0.20 %