Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tipco Tipcolene® CR 6216 - 40% Talc/Mineral Reinforced Polypropylene Copolymer Compound with Controlled Rheology

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® CR 6216 - 40% Talc/Mineral Reinforced Polypropylene Copolymer Compound with Controlled Rheology.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
40% Mineral Reinforced, Controlled Rheology PP CopolymerApplications: Automotive Air DuctsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0085 cm/cm
0.0085 in/in
ASTM D955
Melt Flow 9.0 g/10 min
9.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 75
75
Tensile Strength, Yield 31.4 MPa
4550 psi
ASTM D638
Elongation at Break >= 10 %
>= 10 %
ASTM D638
Flexural Yield Strength 37.0 MPa
5370 psi
ASTM D790
Flexural Modulus 3.14 GPa
455 ksi
ASTM D790
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
ASTM D648