Polymer Property : Flexural Yield Strength = 37.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 37.0 MPa
5370 psi
ASTM D790
NYCOA 715C PA 6
plasticized, high viscosity extrusion grade for monofilament weed eater, fishing lineInformation provided by NYCOA, Inc.
Flexural Yield Strength 37.0 MPa
5370 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP MK0049A PP (Europe-Africa-Middle East)
LNP* STARFLAM* MK0049A is a compound based on Polypropylene resin containing Talc, Flame Retardant. Added features include : Flame Retardant.
Flexural Yield Strength 37.0 MPa
5370 psi
ASTM D790
Tipco Tipcolene® CR 6216 - 40% Talc/Mineral Reinforced Polypropylene Copolymer Compound with Controlled Rheology
40% Mineral Reinforced, Controlled Rheology PP CopolymerApplications: Automotive Air DuctsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Flexural Yield Strength 37.0 MPa
5370 psi
ASTM D790
Tipco Tipcolene® DR 8201 - 20% Talc/Mineral Reinforced, Impact Modified, Polypropylene Copolymer
20% Mineral Reinforced, Impact Modified PP Copolymer BlendApplications: Automotive DashboardsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Flexural Yield Strength 37.0 MPa
5370 psi
ASTM D790
Tipco Tipcolene® FPC 40 PPC - 40% Calcium Carbonate Reinforced Polypropylene Copolymer
40% Calcium Carbonate Filled PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Flexural Yield Strength 37.0 MPa
5370 psi
ASTM D790
Covestro Baydur® SFR-243 Polyurethane Composite RRIM Foam, 15% Milled Glass Filled, MDI-based 2-Component Liquid System
0.25 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – C..
Flexural Yield Strength 37.0 MPa
5370 psi
ASTM D790
Chem Polymer Chemlon 275 Nylon 6, Copolymer Impact Modified
An extrusion grade nylon 6 copolymer that provides excellent melt strength, impact, tensile elongation and flexibility.Data provided by the manufacturer, Chem Polymer.
Flexural Yield Strength 37.0 MPa
5370 psi
DIN 53452
Ineos Nova S-3207 Medium Impact Compact Polystyrene  (discontinued **)
High flow medium impact polystyrene, designed of injection molding of low friction household goods, packaging and toys. It combines low friction properties with excellent (ultrasonic) weldability.A..