Tipco Tipcolene® FX 995 - 10% Talc/Mineral Reinforced, Impact Modified Polypropylene Copolymer Compound with High Flow

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® FX 995 - 10% Talc/Mineral Reinforced, Impact Modified Polypropylene Copolymer Compound with High Flow.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
10% Mineral Reinforced, High Flow, Impact Modified PP CopolymerApplications: Automotive Pillars & TrimsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
ASTM D792
Melt Flow 25 g/10 min
25 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Elongation at Break >= 50 %
>= 50 %
ASTM D638
Flexural Yield Strength 32.0 MPa
4640 psi
ASTM D790
Flexural Modulus 1.80 GPa
261 ksi
ASTM D790
Izod Impact, Notched (ISO) 16.0 kJ/m²
7.61 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 122 °C
252 °F
ASTM D648