Material Notes:
Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer (SBS). Thanks to is broad molecular weight distribution, Finaprene® 602 provides good fluidity properties to the compound while keeping good mechanical properties.ApplicationThanks to its very high crumb porosity Finaprene® 602 is designed for the adhesive and compounding industry.Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
Finaprene 2602 Method
Melt Index of Compound 8.5 g/10 min
8.5 g/10 min
MFI 5kg/200°C; Finaprene 1006 Method
Mechanical Properties Metric English Comments
Hardness, Shore D 36
36
Finaprene 1505 Method
Tensile Strength at Break 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 800 %
800 %
ASTM D638
Chemical Properties Metric English Comments
Styrene Content 40 %
40 %
Finaprene 1004 Method
Butadiene Content 60 %
60 %
Finaprene 1004 Method