Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Toyobo T-751 Nylon, Painting Grade

Category Polymer , Thermoplastic , Nylon
Manufacturer Toyobo
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Toyobo T-751 Nylon, Painting Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Feature: Glass fiber and mineral reinforced, high heat distortion and impact gradesInformation provided by Toyobo Co., Ltd
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Water Absorption 0.70 %
0.70 %
ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm

@Thickness 3.00 mm
0.0050 in/in

@Thickness 0.118 in
Linear Mold Shrinkage, Transverse 0.0090 cm/cm

@Thickness 3.00 mm
0.0090 in/in

@Thickness 0.118 in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Ultimate 63.0 MPa
9140 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Modulus of Elasticity 3.30 GPa
479 ksi
ASTM D638
Flexural Yield Strength 108 MPa
15700 psi
ASTM D790
Flexural Modulus 4.00 GPa
580 ksi
ASTM D790
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C

@Temperature 20.0 °C
22.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 167 °C
333 °F
ASTM D648
Flammability, UL94 HB
HB
unregistered
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Strength 21.0 kV/mm

@Thickness 2.00 mm
533 kV/in

@Thickness 0.0787 in
ASTM D149
Arc Resistance 120 sec
120 sec
ASTM D495
Users viewing this material also viewed the following: