Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | ISO 294 |
Polyplastic Armlen® PP MF 15-3 FR Polypropylene Homopolymer, Mineral Filled Flame retardant, RoHS compliantInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | 380°C nozzle, 190°C tool; ISO 294-4 |
Victrex® PEEK 450GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm @Thickness 2.00 mm |
0.0090 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66
(Unverified Data**) Zytel® FR70M30V0 BK010 is a 30% mineral reinforced, flame retardant, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4 |
DSM Akulon® Ultraflow™ K-FG0 Nylon 6-50% Glass Reinforced (European and Asian Grade) (Dry)
(discontinued **)& The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4 |
DSM Akulon® Ultraflow™ K-FHGM44 Nylon 6-40% Glass and Mineral Reinforced (European and Asian Grade) (Dry)
(di The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4, 2577 |
Kuraray Genestarâ„¢ G1350A-M42 Nylon, 35% Glass Filled 35% Glass reinforced injection grade. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment.Main Features:Hydrolysis resistanceHeat resista.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4 |
Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product off.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RFN169 PA 66 LNP* LUBRICOMP* RFN169 is a compound based on Nylon 66 containing 30% Glass Fiber, 5% MOS2. Added features of this grade include: Wear Resistant, Flame Retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RF007ES PA 66 LNP* THERMOCOMP* RF007ES is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Heat Stabilized, Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ASTM D955 |
Teknor Apex Telcar® TL-1273A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | ISO DIS 294-4 |
Wellman Wellamid® GFT1628-BK 17% Glass Fiber Reinforced, Impact Modified Nylon 66 Description: Glass Fiber Reinforced, Impact Modified Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | |
Toyobo VYLOPET® EMC320R Polyester Resin VYLOPET® is a polyester resin developed specifically for injection molding. Polyester resins have excellent heat resistance, rigidity, chemical resistance, and electric properties. Grade EMC320R ha.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | |
Toyobo Vylopet® EMC330K Glass Reinforced Polyester, Easy Molding Grade HB UL-94 classApplications: General and high rigidity componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, c.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | |
Toyobo VYLOPET® EMC341 Injection Molding Polyester Resin, Hydrolysis Resistant Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm @Thickness 4.00 mm |
0.0090 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6600 CF10 HWCP 10% Carbon Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® CE15330 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® CE15330 NC010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® 70G43HSLA BK099 Nylon 66
(Unverified Data**) 43% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G43HSLA BK099 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont .. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® HTN 92G35DH2 BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G35DH2 BK083 is a 35% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | Eurotec |
Eurotec® Tecopet® PT70 GR30 NL100 XD70 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), long-term heat stabilized, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-27 CF10 Polyamide 6 10% Carbon Fiber - Antistatic and Electroconductive Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO 2577 |
BASF Ultramid® S3EG6 Balance 30% Glass Filled PA 610 (Dry) Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. .. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | Dry; ASTM D2863 |
Asahi Kasei Leona® 13G25 25% Glass Filled Nylon 66 Enhanced strength, stiffness and durability; with 25% GF.Applications:Automotive parts Information provided by Asahi Kasei |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4 |
Akro-Plastic Akromid® B3 GF 40 (2474) PA 6 Dry, 40% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO Data |
BASF Capron® 8234G 44% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8234G is a 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is .. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Minlon® 11C40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66 Minlon 11C40 NC010 is a 40% mineral reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.011 cm/cm @Thickness 3.18 mm |
0.0090 - 0.011 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | |
LATI Latilub 66-15ST G/30 PA66, 30% Glass Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). Silicone / PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm @Diameter 2.00 mm |
0.0090 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, Conditioned Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm @Thickness 2.00 mm |
0.0090 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Dry as Molded Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.018 cm/cm | 0.0090 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 315 PBT (Europe-Africa-Middle East) VALOX 315 is compliant with food contact regulations acc. to EC Reg. No. 10/2011. VALOX 315 can be applied for injection moulding and extrusion puposes. |