Material Notes:
TRA-BOND 2101 is a medium viscosity epoxy formulation recommended for laminating, bonding, repair and other adhesive applications where the combination of its superior structural, mechanical and electrical performance properties are required. This two-part adhesive easily mixes and cures at room temperature, and develops strong, durable, tough bonds to most clean, dry material surfaces - including metals, ceramics, glass and glass fabrics, wood leather, and many rigid plastics. The fully cured TRA-BOND 2101 bonds are good electrical insulators which also provide excellent resistance to weather, galvanic action, many mild acids and alkalis, salt solution, petroleum solvents, lubricating oil, gasoline, jet fuels, alcohol, and many other organic and inorganic materials.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Mixed
Solids Content 100 %
100 %
Reactive Solids Content
Viscosity 19000 cP

@Temperature 25.0 °C
19000 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Adhesive Bond Strength 22.8 MPa
3300 psi
Lap shear, alum to alum
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
Thermal Properties Metric English Comments
CTE, linear 55.0 µm/m-°C

@Temperature 20.0 °C
30.6 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 135 °C
275 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 62.0 °C
144 °F
Ultimate Tg
Electrical Properties Metric English Comments
Volume Resistivity 6.00e+15 ohm-cm
6.00e+15 ohm-cm
5.00e+9 ohm-cm

@Temperature 100 °C
5.00e+9 ohm-cm

@Temperature 212 °F
Dielectric Constant 4.3

@Frequency 1000 Hz
4.3

@Frequency 1000 Hz
Dielectric Strength 14.6 kV/mm
370 kV/in
Dissipation Factor 0.020

@Frequency 1000 Hz
0.020

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 30 min
30 min
Descriptive Properties Value Comments
Color Clear, Slight Haze
Mix Ratio, parts by weight 100/25
Resin/Hardener