Tra-Con Tra-Bond 546S05 Dual-Cure Acrylate

Category Polymer , Adhesive , Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 546S05 Dual-Cure Acrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND 546S05 is a dual cure (UV/heat) acrylate featuring excellent adhesion to glass. Ultimate Tg attained and shadowed areas cured with 15 minute exposure to 100-120°C.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Cured
Viscosity 5500 cP
5500 cP
Mixed (cp #40, 2.5 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 86
86
Adhesive Bond Strength 6.89 MPa
1000 psi
Lap shear, adhesion to glass, minimum
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 85.0 °C
185 °F
Ultimate Tg, 10°C/min; TMA
Processing Properties Metric English Comments
Cure Time 0.0833 - 0.167 min
0.00139 - 0.00278 hour
UV exposure
Descriptive Properties Value Comments
Color Light Red
Uncured
Transparent Yellow
Cured