Material Notes:
TRA-BOND 724-14C premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong, resilient bonds to a wide variety of substrates, including aluminum, solder, nylon, mylar and steel. Adhesive strength is maintained even in cryogenic conditions. This resilient adhesive can also be used for tacking wires and as a protective coating. TRA-BOND 724-14C adhesive exhibits good dielectric properties. There are several cure options, including curing at room temperature. It contains a fluorescent trace for inspection purposes.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Mixed
Viscosity 500000 cP
500000 cP
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
Adhesive Bond Strength 11.7 MPa
1700 psi
Lap shear, alum to alum
Peel Strength 3.51 kN/m
20.0 pli
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
Dielectric Constant 7.0

@Frequency 1000 Hz
7.0

@Frequency 1000 Hz
Processing Properties Metric English Comments
Extrusion Rate 0.250 g/min
0.250 g/min
15 gauge needle @ 80 psi
Cure Time 60.0 min

@Temperature 93.0 °C
1.00 hour

@Temperature 199 °F
180 min

@Temperature 74.0 °C
3.00 hour

@Temperature 165 °F
4320 min

@Temperature 25.0 °C
72.0 hour

@Temperature 77.0 °F
Shelf Life 3.00 Month

@Temperature -40.0 °C
3.00 Month

@Temperature -40.0 °F
Descriptive Properties Value Comments
Color Amber
Working Life minutes 30
At 25°C
Users viewing this material also viewed the following: