Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Eccobond®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Eccobond® TP 50 Two-Component Low Temperature Performance Silicone Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Emerson & Cuming TP 50 Eccobond® Two-Component Low Temperature Performance Silicone AdhesiveFilled, RTV silicone rubber, paste adhesive. Room temperature cure. Very flexible. Color coded for ease of use. Requires use of a primer (S-11). Recommended for seam sealing, caulking, bonding or application to vertical surfaces. Mix ratio of 100:9 Cure Type: Room Temp or Heat Bonding Type: Silicone
Physical Properties Metric English Comments
Density 1.87 g/cc
0.0676 lb/in³
Mechanical Properties Metric English Comments
Adhesive Bond Strength 0.689 MPa
100 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 230 °C
446 °F
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 120 °C
1.00 hour

@Temperature 248 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Red
Viscosity Thixotropic Paste