Trelleborg Emerson & Cuming Stycast® 2760 Two-Component Easy Mix Ratio Encapsulant

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Stycast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Stycast® 2760 Two-Component Easy Mix Ratio Encapsulant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, thermal and mechanical shock resistance, and thermal conductivity.Emerson & Cuming 2760 Stycast® Two-Component Easy Mix Ratio EncapsulantMix Ratio by weight = 100:50Good Chemical ResistanceThermally ConductiveFilled Cure Type: Room Temp or Heat Bonding Type: Epoxy/Polyurethane
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
Viscosity 18000 cP

@Temperature 25.0 °C
18000 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Thermal Properties Metric English Comments
CTE, linear 122 µm/m-°C

@Temperature 20.0 °C
67.8 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.600 W/m-K
4.16 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Dielectric Constant 4.0

@Frequency 1e+6 Hz
4.0

@Frequency 1e+6 Hz
Dielectric Strength 17.7 kV/mm
450 kV/in
Processing Properties Metric English Comments
Cure Time >= 120 min
>= 2.00 hour