Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing 30% Mixed Glass, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | |
3M Dyneon™ Aflas® FA-150L PTFE Fluoroelastomer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® FR515 BK507 PET
(Unverified Data**) Rynite® FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm(0.03in). Has a 140C temp index. Excellent balance of electr.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
Pasargad Polymer Peyvand Pasamid 3P-H1150B Nylon 6, 50% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36 PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL-4036 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | |
LATI Latiohm 73-09 PD01 G/20 POM, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyoxymethylene (POM). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP KL005 Acetal Copolymer (Asia Pacific) LNP* LUBRICOMP* KL005 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXC PPA (Asia Pacific) LNP* Lubricomp* UFL36SXC is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXC PPA (Asia Pacific) LNP* Lubricomp* UFL36SXC is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXQ PPA (Asia Pacific) LNP* Lubricomp* UFL36SXQ is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
Techmer ES HiFill® HTN GF HS L High Temp Nylon 50% Glass Filled Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Heat ResistanceInformation provided by TP Composit.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
Polyplastics Duranex® C5330 Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | DIN 53479 |
Polyram PB302G50 Nylon 6, 50% Glass Fiber 50% glass fiber reinforced, UV and heat stabilized polyamide approved and listed by W.R.C potable water and NSF/ANSI61 internationalInformation provided by Polyram Ram On Ind. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | DIN 53479 |
Polyram PlusTek PA303G50 Nylon 6.6, 50% Glass Fiber 50% glass fiber reinforced, heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | Relative Density; ISO 1183 |
Vyncolit X6151 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Highest impact, high strain to failure, glycol resistant.USES: Water pumps and water pump .. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | |
Trelleborg Emerson & Cuming Stycast® G-508-1 One-Component Epoxy Flame Retardant Encapsulant Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conduc.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
Plenco 4300 Phenolic, Granular, Transfer Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
DSM Arnite® TV4 461 (PBT+PET)-GF30 30% Glass Reinforced |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
Eurostar Staramide PB00A PA6, 50% Glass Bead Filled, Injection Molded Staramide PB00A is a 50% Glass Bead Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
CP-Polymer-Technik Wellamid® 6000 GS 50 HWUVCP 50% Glass Sphere Filled Nylon 6, UV Stabilized Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Density | 1.55 - 1.59 g/cc | 0.0560 - 0.0574 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 82 Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® E126 PET Polyester, 30% Glass Reinforced PET Polyester, economy grade with 30% glass reinforcement.Data provided by the manufacturer |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
Chem Polymer Durlex 730 G PBT, 30% Glass Fiber Reinforced A lubricated 30% glass reinforced PBT offering a balance of dimensional stability, tensile strength and high temperature performance.Data provided by the manufacturer, Chem Polymer. |
|||
Density | 1.55 g/cc @Temperature 25.0 °C |
0.0560 lb/in³ @Temperature 77.0 °F |
Liquid |
Asahi Glass ASAHIKLIN AK-225DH Hydrochlorofluorocarbon Solvent AK-225DH was developed as a solvent dewatering and drying system to remove water from the surface of various parts and assemblies. AK-225DH is a mixture of AK-225 and a drying agent to give it rapid.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
BASF Ultradur B 4406 G4 PBT Description: Is a PBT, flame-retardant injection-molding grades, with 20% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
Chevron Phillips Xtel® XK2240 Polyphenylene Sulfide Alloy
(discontinued **) Natural Color Polyphenylene Sulfide AlloyXtel™ XK2240 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength with an unique blend of tough.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
Lanxess Pocan® B 3235 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183/A |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | |
3M Dyneon™ Aflas® FA-150P PTFE Fluoroelastomer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium.. |