Trelleborg Emerson & Cuming Stycast® TU-906 Two-Component Polyurethane Flexible Encapsulant

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced , Polyurethane, TS
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Stycast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Stycast® TU-906 Two-Component Polyurethane Flexible Encapsulant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Emerson & Cuming TU-906 Stycast® Two-Component Polyurethane Flexible EncapsulantDescriptionGood thermal shock and moisture resistance. Good chemical resistance. Low viscosity. Mix Ratio (by weight) = 100:400 Cure Type: Room Temp or Heat Bonding Type: Polyurethane
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
Viscosity 3100 cP

@Temperature 25.0 °C
3100 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Cure Time >= 120 min
>= 2.00 hour