Material Notes:
All information provided by Trelleborg
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
Tensile Strength, Yield 16.0 MPa
2320 psi
Elongation at Break 600 %
600 %
Tear Strength 27.0 kN/m
154 pli
Abrasion 90
90
mm<sup>3</sup>; 5 N Load
Compression Set 35 %

@Temperature 70.0 °C,
Time 79200 sec
35 %

@Temperature 158 °F,
Time 22.0 hour
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 85.0 °C
185 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Descriptive Properties Value Comments
Color Black