Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 27.0 kN/m | 154 pli | post cured- 2 hours at 177°C; Die B |
Multibase SILASTIC® C7-4550 TBPB Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 27.0 kN/m | 154 pli | D624 |
Polykemi AB POLYelast TPE E706 Thermoplastic Elastomer, EPDM-based Information provided by Polykemi AB |
|||
Tear Strength | 27.0 kN/m | 154 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 221-73 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Tear Strength | 27.0 kN/m | 154 pli | Die B, post cured- 8 hours at 177°C; ASTM D624 |
Multibase C6-530 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 27.0 kN/m | 154 pli | |
Trelleborg B568 High Quality Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tear Strength | 27.0 kN/m | 154 pli | |
Trelleborg E645 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tear Strength | 27.0 kN/m | 154 pli | |
Trelleborg E646 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tear Strength | 27.0 kN/m | 154 pli | |
Trelleborg R431 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 27.0 kN/m | 154 pli | |
Trelleborg R547 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | >= 27.0 kN/m | >= 154 pli | |
Trelleborg Offshore Vikotherm™ 73785 Insulative Elastomer Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res.. |
|||
Tear Strength | 27.0 kN/m | 154 pli | |
Trelleborg E647 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tear Strength | 27.0 kN/m | 154 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 40A, Non-Black Sulfur Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 27.0 kN/m | 154 pli | ASTM D624 |
ELASTO UK Dryflex® 400601S SBS Based Material, 60A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Tear Strength | 27.0 kN/m | 154 pli | ASTM D624 |
ELASTO UK Dryflex® 402601S SBS Based Material, 60A Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Tear Strength | 27.0 kN/m | 154 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 201-73 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Tear Strength | 27.0 kN/m | 154 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 271-73 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Tear Strength | 27.0 kN/m @Thickness 0.760 mm |
154 pli @Thickness 0.0299 in |
Split tear strength; extruded sheet; ASTM D-1938 |
BASF Elastollan® 1175A10W Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Tear Strength | 27.0 kN/m | 154 pli | Perpendicular to flow; ISO 34-B |
AlphaGary Evoprene™ LF 6150 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Tear Strength | 27.0 kN/m | 154 pli | ISO 34-B |
AlphaGary Evoprene™ 075 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Tear Strength | 27.0 kN/m | 154 pli | ISO 34-B |
AlphaGary Evoprene™ 076 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Tear Strength | 27.0 kN/m | 154 pli | 73°C, Die C; ASTM D624 |
ExxonMobil Geolast® 701-80W183 Thermoplastic Elastomer A soft, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic.. |
|||
Tear Strength | 27.0 kN/m | 154 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 40A, Non-Black Sulfur Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |