Trimay® Wear Plate TWP57 Chromium-based Flux Cored Weld Wire & Electrode

Category Metal , Ferrous Metal , Alloy Steel
Manufacturer Trimay® Wear Plate Ltd
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trimay® Wear Plate TWP57 Chromium-based Flux Cored Weld Wire & Electrode.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TWP57 is a chromium-based flux cored wire electrode used to protect equipment and parts from heavy wear and mild-to-moderate direct impact. TWP57 has a compatible compostion that allows it to be applied on a wide array of materials and it maintains good Rockwell Hardness (HRc) and wear ability at elevated temperatures.Key Performance Characteristics: Heavy abrasion and mild/moderate impact resistance, Compatible composition for welding, Hardness increase on underlying layer(s), Good hardness at elevated temperaturesApplications: TWP57 can be overlain on carbon steel, manganese base materials and mild or alloy steels. The maximum recomended deposit thickness of TWP56 is 2 - 3 layers, or 1/4” (6.35mm). TWP57 is used to cover exposed bolts and seams for installation of T156 wear plate and parts, as well as for small area lining of heavy wearing parts and equipment such as the front lip ‘bullnose’ of asphalt screeds.Information provided by Trimay®
Mechanical Properties Metric English Comments
Hardness, Rockwell C 59
59
Wire, layer 1
61 - 63
61 - 63
Electrodes
63
63
Wire, layer 2
Component Elements Properties Metric English Comments
Carbon, C <= 5.0 %
<= 5.0 %
Chromium, Cr <= 30 %
<= 30 %
Iron, Fe >= 62 %
>= 62 %
Manganese, Mn <= 1.5 %
<= 1.5 %
Silicon, Si <= 1.5 %
<= 1.5 %
Descriptive Properties Value Comments
Available Sizes: Electrode 3.25
[mm]
4
[mm]
5
[mm]
Available Sizes: Wire 1.6
[mm], cored wire
2.4
[mm], cored wire
2.8
[mm], cored wire
Packaging: Electrode 3.5
[mm] 4.5kg sleeves (4 sleeves=1 box)
4
[mm] 4.5kg sleeves (4 sleeves=1 box)
5
[mm] 5kg sleeves (4 sleeves=1 box)
Packaging: Wire 1.6
[mm], 25kg spools
2.4
[mm], 25kg spools
2.8
[mm], 25kg spools