Material Notes:
Specialties: High viscosity Nylon 6/66 Copolymer, High transparent and tenacity, Higher drawing ratio can be achieved for superior line strengthApplications: Small-medium size sport fishing line Information provided by UBE.
Physical Properties Metric English Comments
Fiber Count 1470 dtex
1320 denier
Mechanical Properties Metric English Comments
Elongation at Break 38 %
38 %
Line Elongation
38 %
38 %
Knot Elongation
Tenacity 0.618 N/tex
7.00 g/denier
Knot Strength
0.644 N/tex
7.30 g/denier
Line Strength
1.41 N/tex
16.0 g/denier
Tensile Modulus
Thermal Properties Metric English Comments
Shrinkage 23 %
23 %
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified