Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 1.41 N/tex | 16.0 g/denier | Tensile Modulus |
UBE 5033T Nylon 6/66 Monofilament (Drawing Ratio=5) Specialties: High viscosity Nylon 6/66 Copolymer, High transparent and tenacity, Higher drawing ratio can be achieved for superior line strengthApplications: Small-medium size sport fishing line Inf.. |