Like Foamfrax RG, Foamfrax® RG Plus combines refractory ceramic fiber, refractory cement, and a high-temperature binder solution that can be combined in the field using the uniqued Foamfrax process. The resultant product form, which is rated to 2300°F, is a high-density, ceramic fiber based material ideally suited for low-density working linings. Foamfrax RG Plus can be gunned easily around a variety of refractory anchor systems and air sets within 24 hours. For full thickness applications of this material, all established installation guidelines for Foamfrax full thickness linings must be adhered to. This includes choosing the proper anchoring system for the applications, troweling the hot face smooth, and scoring on a maximum of 2' x 2' centers.Principal ApplicationsBackup behind brick, plastic, refractory, and castableAnnealing furnace basesDuct, flue, and stack liningsHeat treat furnace, kiln car decksIncinerator floors, process heatersInformation Provided by Unifrax I LLC
Physical Properties Metric English Comments
Density 0.352 - 0.449 g/cc
0.0127 - 0.0162 lb/in³
Dry
0.368 - 0.481 g/cc

@Treatment Temp. 1260 °C,
Time 86400 sec
0.0133 - 0.0174 lb/in³

@Treatment Temp. 2300 °F,
Time 24.0 hour
Fired
Loss On Ignition 6.0 - 9.0 %

@Treatment Temp. 1260 °C,
Time 86400 sec
6.0 - 9.0 %

@Treatment Temp. 2300 °F,
Time 24.0 hour
Mechanical Properties Metric English Comments
Modulus of Rupture 0.172 - 0.241 GPa
25.0 - 35.0 ksi
Dry
0.103 - 0.172 GPa

@Treatment Temp. 1260 °C,
Time 86400 sec
15.0 - 25.0 ksi

@Treatment Temp. 2300 °F,
Time 24.0 hour
Fired
Compressive Strength 0.276 - 0.345 MPa
40.0 - 50.0 psi
Cold Crush Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1260 °C
2300 °F
Continuous
Shrinkage 3.0 %

@Treatment Temp. 1260 °C,
Time 86400 sec
3.0 %

@Treatment Temp. 2300 °F,
Time 24.0 hour
Linear
Descriptive Properties Value Comments
Appearance Brown Fibrous/Cement Mixture
Set Time (Hours) 24