Physical Properties Metric English Comments
Density 0.352 g/cc
0.0127 lb/in³
Pyrotek M-14 Compressible/Insulating Boards
ApplicationsSiphon gaskets Trough and ladle linings Tundishes Mill board substitute AdvantagesResistant to chemical attack Excellent thermal shock resistance Slightly flexible Moderately compressibl..
Density 0.352 g/cc
0.0127 lb/in³
Fired Density at 1500°F
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M607 Moldable
Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or ..
Density 0.352 g/cc
0.0127 lb/in³
Nominal
Unifrax Fiberfrax® Duraboard® 500ES Ceramic Fiber Board
Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard ..
Density 0.352 - 0.449 g/cc
0.0127 - 0.0162 lb/in³
Dry
Unifrax Foamfrax® Isofoam® RG Insulation
Foamfrax® RG (Refractory Grade) Insulation is an extension of the Foamfrax Insulation product line. Foamfrax RG Insulation is a combination of refractory ceramic fiber or soluble fiber, refractory..
Density 0.352 - 0.449 g/cc
0.0127 - 0.0162 lb/in³
Dry
Unifrax Foamfrax® RG Insulation
Foamfrax® RG (Refractory Grade) Insulation is an extension of the Foamfrax Insulation product line. Foamfrax RG Insulation is a combination of refractory ceramic fiber or soluble fiber, refractory..
Density 0.352 - 0.449 g/cc
0.0127 - 0.0162 lb/in³
Dry
Unifrax Foamfrax® RG Plus Insulation
Like Foamfrax RG, Foamfrax® RG Plus combines refractory ceramic fiber, refractory cement, and a high-temperature binder solution that can be combined in the field using the uniqued Foamfrax process..
Density 0.352 - 0.417 g/cc
0.0127 - 0.0150 lb/in³
Engineered Syntactic Systems BZ-24 Deep Water Syntactic Foam
Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having..
Density 0.352 - 0.417 g/cc
0.0127 - 0.0150 lb/in³
Engineered Syntactic Systems MZ-24 Deep Water Syntactic Foam
Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having..
Density <= 0.352 g/cc
<= 0.0127 lb/in³
Engineered Syntactic Systems SF-22 Subsea Macrosphere Syntactic Void Filler
In applications where density is critical, the four part SF-22 kit is used. This system utilizes fiber reinforced epoxy macrospheres in combination with the standard microsphere syntactic to provide..