Material Notes:
Insulfrax® Paper is an evolutionary product which is manufactured by forming Insulfrax Fiber in a nonwoven matrix. These fibers are randomly oriented during manufacturing and then held in place with a latex binder system. A specialized paper-making process is utilized to form uniform lightweight, flexible materials, including Insulfrax Paper.Insulfrax Fiber, utilized in Insulfrax Paper, in based upon a calcium, magnesium, silicate (CMS) chemistry. This CMS fiber chemistry has been successfully used to solve a variety of application problems from 800°F (427°C) up to 2012°F (1100°C). In addition to high temperature resistance, Insulfrax Fiber meets European regulatory requirements (Directive 97/69/EC).The calcium, magnesium, silicate chemistry of Insulfrax Fiber provides superior wetting resistance to molten aluminum alloys. Testing with corrosive aluminum alloys at elevated temperatures has proven that Insulfrax is superior to traditional alumina/silica refractory ceramic fibers.Insulfrax Paper will generate small amounts of smoke and trace element outgassing during initial exposure to temperatures above 450°F (232°C).AdvantagesHigh-temperature stability up to 2012°F (1100°C)Meets European regulatory requirementsSuperior wetting resistance to molten aluminumLow thermal conductivityFlexibilityEasy to wrap, shape, or cutApplicationsAutomotive and aerospace heat shieldsGaskets for ovens, stoves, heaters, and other appliancesNonferrous ingot mold linersRefractory backup insulation in ladles, glass tanks, and other high-temperature furnacesParting medium in brazing and solderingMolten aluminum transfer systemsInformation Provided by Unifrax I LLC
Physical Properties Metric English Comments
Density 0.144 - 0.160 g/cc
0.00521 - 0.00579 lb/in³
Loss On Ignition <= 12 %
<= 12 %
(Wt.) including binder
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 0.248 MPa
>= 36.0 psi
Average
Thermal Properties Metric English Comments
Melting Point 1310 °C
2390 °F
Maximum Service Temperature, Air 1100 °C
2010 °F
Recommended Operating Temperature
Shrinkage <= 4.0 %

@Temperature 1100 °C,
Time 86400 sec
<= 4.0 %

@Temperature 2010 °F,
Time 24.0 hour
Descriptive Properties Value Comments
Color White
Fiber Index (% Wt) >50
Temperature Grade (°C) 1260