Material Notes:
Carbon black Chezacarb is manufactured by gasification of heavy petroleum residues by partial oxidation in Shell reactors. It is produced in the form of pellets of size 0,5 - 2,5 mm. Product is not classified as dangerous according to EC Directives.Carbon black Chezacarb is made in three sorts: A+, A and B. There are suitable mostly for modification of conductance and heat conductivity in plastics and rubber, due to their high specific surface and high poresity.Information provided by Unipetrol RPA
Physical Properties Metric English Comments
Bulk Density <= 0.112 g/cc
<= 0.00405 lb/in³
pH 6.5 - 9.5
6.5 - 9.5
Specific Surface Area >= 800 m²/g
>= 800 m²/g
by nitrogen absorption
Iodine Absorption Number 950 - 1250
950 - 1250
mg/g
Ash <= 1.7 %
<= 1.7 %
Evaporation Loss <= 0.80 %
<= 0.80 %
Component Elements Properties Metric English Comments
Iron, Fe <= 0.18 %
<= 0.18 %
Nickel, Ni <= 0.25 %
<= 0.25 %
Sulfur, S <= 0.60 %
<= 0.60 %
Vanadium, V <= 0.50 %
<= 0.50 %
Electrical Properties Metric English Comments
Electrical Resistivity <= 150 ohm-cm
<= 150 ohm-cm
Descriptive Properties Value Comments
Composition max. 20
DBP Absorption (ml/100g) 380-460
Material Fines content