Material Notes:
Unleaded mogases represent the hydrocarbon blend usually boiling within 20 to 215°C, obtainted from crude oil through distillation and refining processes. They may contain additives that enhance their application characteristics, e.g. oxygenous components, detergents, antiknock, antioxidative and other additives. Unleaded mogases are mainly applied in spark-ignition engines of road motor vehicles. They are not allowed to be used in vehicles operating within confined workspaces. Unleaded mogases are designed especially for modern-type spark-ignition engines equipped with catalyst and lambda probe controlled.Information provided by Unipetrol RPA
Physical Properties Metric English Comments
Density 0.725 - 0.775 g/cc

@Temperature 15.0 °C
0.0262 - 0.0280 lb/in³

@Temperature 59.0 °F
Vapor Pressure 0.450 - 0.600 bar
337 - 450 torr
Reid Vapor Pressure, Summer
0.600 - 0.900 bar
450 - 675 torr
Reid Vapor Pressure, Winter
Evaporation Loss 20 - 48 %
20 - 48 %
22 - 50 %

@Temperature 70.0 °C
22 - 50 %

@Temperature 158 °F
Summer
46 - 71 %

@Temperature 70.0 °C
46 - 71 %

@Temperature 158 °F
Winter
>= 75 %

@Temperature 100 °C
>= 75 %

@Temperature 212 °F
Component Elements Properties Metric English Comments
Lead, Pb <= 0.00050 %
<= 0.00050 %
Sulfur, S 0.0050 %
0.0050 %
Descriptive Properties Value Comments
Appearance transparent and clear
Aromatics Content (%), max 35
Benzene Content (%), max 1
Mechanical Impurities and Water % none
Octane Number MON, min 82
Octane Number RON, min 95
Resinous Content, mg/100cm³, max 5
Volatility Index (April and October), max 1150