Material Notes:
Offers exceptional machinability and excellent surface finishes, but limited strength and wear resistance. Noise and vibration damping are excellent in this grade.Unibar-200 is not suitable for hardening applications.Information provided by United Cast Bar Ltd.
Physical Properties Metric English Comments
Density 7.30 g/cc
0.264 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 120 - 200

@Load 3000 kg
120 - 200

@Load 6610 lb
10 mm ball
Tensile Strength 115 MPa

@Diameter 150 - 300 mm
16700 psi

@Diameter 5.91 - 11.8 in
130 MPa

@Diameter 80.0 - 150 mm
18900 psi

@Diameter 3.15 - 5.91 in
155 MPa

@Diameter 40.0 - 80.0 mm
22500 psi

@Diameter 1.57 - 3.15 in
180 MPa

@Diameter 20.0 - 40.0 mm
26100 psi

@Diameter 0.787 - 1.57 in
Component Elements Properties Metric English Comments
Carbon, C 2.95 - 3.45 %
2.95 - 3.45 %
Iron, Fe 92.63 - 94.26 %
92.63 - 94.26 %
as balance
Manganese, Mn 0.55 - 0.75 %
0.55 - 0.75 %
Phosphorous, P 0.10 - 0.20 %
0.10 - 0.20 %
Silicon, Si 2.1 - 2.9 %
2.1 - 2.9 %
Sulfur, S 0.040 - 0.070 %
0.040 - 0.070 %