Weather resistant, noncoating, external exposure-compatibleInformation provided by Unitika Ltd.
Physical Properties Metric English Comments
Density 1.66 g/cc
0.0600 lb/in³
ASTM D792
Water Absorption 1.05 %
1.05 %
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 136 MPa
19700 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Strength 175 MPa
25400 psi
ASTM D790
Flexural Modulus 11.0 GPa
1600 ksi
ASTM D790
Izod Impact, Notched 0.630 J/cm
1.18 ft-lb/in
ASTM D256