Universal Wire Works 505 E8018-B8 Stainless Steel Electrode

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 505 E8018-B8 Stainless Steel Electrode.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Universal 505 electrodes deposit 9% chromium 1% molybdenum deposits in applications that are primarily pipe, tube and castings. Type 505 is an air hardening alloy and as such requires both a preheat and stress relief for satisfactory results.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 414 MPa
60000 psi
Elongation at Break 20 %
20 %
Component Elements Properties Metric English Comments
Carbon, C 0.10 %
0.10 %
Chromium, Cr 9.5 %
9.5 %
Iron, Fe 87.1 %
87.1 %
As Remainder
Manganese, Mn 1.0 %
1.0 %
Molybdenum, Mo 1.0 %
1.0 %
Nickel, Ni 0.40 %
0.40 %
Silicon, Si 0.90 %
0.90 %