Material Notes:
Alloy 61 is used for TIG, MIG, and submerged-arc welding of Nickel 200 and 201, and for overlaying on steel. There is a reaction of carbon with titanium during the welding process so there is a low level of free carbon, which permits Alloy 61 to be used on Nickel 201. Dissimilar welding applications of Alloy 61 include: joining Monel type alloys and copper-nickel alloys to carbon steels, Inconel and Incoloy type alloys to copper-nickel alloys and Monel alloys.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 414 MPa
60000 psi
Elongation at Break 20 %
20 %
Component Elements Properties Metric English Comments
Aluminum, Al <= 1.5 %
<= 1.5 %
Carbon, C <= 0.15 %
<= 0.15 %
Copper, Cu <= 0.25 %
<= 0.25 %
Iron, Fe <= 1.0 %
<= 1.0 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Nickel, Ni >= 93 %
>= 93 %
Other <= 0.50 %
<= 0.50 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Silicon, Si <= 0.75 %
<= 0.75 %
Sulfur, S <= 0.015 %
<= 0.015 %
Titanium, Ti 2.0 - 3.5 %
2.0 - 3.5 %