Universal Wire Works 625 Nickel Alloy Welding Wire

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 625 Nickel Alloy Welding Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alloy 625 is used for TIG, MIG and submerged-arc welding of Inconel type alloys 601 and 625, Incoloy type alloy 800, as well as overlaying on steel and joining 9% nickel steel. Alloy 625 can be used for welding a variety of dissimilar joints including Inconel type alloys, Incoloy type alloys, stainless steels, low alloy steels and carbon steels. Alloy 625 is also available in a
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 758 MPa
110000 psi
Elongation at Break 30 %
30 %
Component Elements Properties Metric English Comments
Aluminum, Al <= 0.40 %
<= 0.40 %
Carbon, C <= 0.10 %
<= 0.10 %
Chromium, Cr 20 - 23 %
20 - 23 %
Cobalt, Co <= 1.0 %
<= 1.0 %
Copper, Cu <= 0.50 %
<= 0.50 %
Iron, Fe <= 5.0 %
<= 5.0 %
Manganese, Mn <= 0.50 %
<= 0.50 %
Molybdenum, Mo 8.0 - 10 %
8.0 - 10 %
Nickel, Ni >= 58 %
>= 58 %
Niobium, Nb (Columbium, Cb) 3.15 - 4.15 %
3.15 - 4.15 %
Other <= 0.50 %
<= 0.50 %
Phosphorous, P <= 0.020 %
<= 0.020 %
Silicon, Si <= 0.50 %
<= 0.50 %
Sulfur, S <= 0.015 %
<= 0.015 %
Titanium, Ti <= 0.40 %
<= 0.40 %