Universal Wire Works 82 Nickel Alloy Welding Wire

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 82 Nickel Alloy Welding Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alloy 82 is used for TIG, MIG and submerged-arc welding of Inconel type alloys 600 and 601, Incoloy type alloy 800 and welding the clad side of steel clad with nickel chromium alloy. Dissimilar metals welding applications include: joining stainless steels to carbon steel, Nickel 200, Monel type 400; Inconel and Incoloy type alloys to stainless steels, carbon steel, Nickel 200 and Monel type 400.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 552 MPa
80000 psi
Elongation at Break 30 %
30 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.10 %
<= 0.10 %
Chromium, Cr 18 - 22 %
18 - 22 %
Cobalt, Co <= 0.12 %
<= 0.12 %
Copper, Cu <= 0.50 %
<= 0.50 %
Iron, Fe <= 3.0 %
<= 3.0 %
Manganese, Mn 2.5 - 3.5 %
2.5 - 3.5 %
Molybdenum, Mo 0.50 %
0.50 %
Nickel, Ni >= 67 %
>= 67 %
Niobium, Nb (Columbium, Cb) 2.0 - 3.0 %
2.0 - 3.0 %
Other <= 0.50 %
<= 0.50 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Sulfur, S <= 0.015 %
<= 0.015 %
Tantalum, Ta <= 0.30 %
<= 0.30 %
Titanium, Ti <= 0.75 %
<= 0.75 %