Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Universal Wire Works 901 (AMS 5660) Nickel Alloy Filler Metal

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 901 (AMS 5660) Nickel Alloy Filler Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alloy 901 is a corrosion and heat resistant nickel-base alloy designed for gas tungsten arc and gas metal arc welding. Alloy 901 is used primarily for parts, such as turbine rotors, shafts and buckets or blades requiring high strength up to 1400°F (760°C) and oxidation resistance up to 1600°F (871°C).Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 1030 MPa
>= 150000 psi
Tensile Strength, Yield >= 689 MPa

@Strain 0.200 %
>= 100000 psi

@Strain 0.200 %
Elongation at Break >= 12 %
>= 12 %
4D
Component Elements Properties Metric English Comments
Aluminum, Al <= 0.35 %
<= 0.35 %
Boron, B <= 0.020 %
<= 0.020 %
Carbon, C <= 0.10 %
<= 0.10 %
Chromium, Cr 13 %
13 %
Copper, Cu <= 0.50 %
<= 0.50 %
Iron, Fe >= 32.4 %
>= 32.4 %
As Remainder
Manganese, Mn <= 1.0 %
<= 1.0 %
Molybdenum, Mo 6.0 %
6.0 %
Nickel, Ni 43 %
43 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Silicon, Si <= 0.60 %
<= 0.60 %
Sulfur, S <= 0.030 %
<= 0.030 %
Titanium, Ti 3.0 %
3.0 %
Users viewing this material also viewed the following: