Universal Wire Works AMS 4764 Silver Brazing Filler Metal

Category Metal , Nonferrous Metal , Copper Alloy , Solder/Braze Alloy
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works AMS 4764 Silver Brazing Filler Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Universal Wire Works for their line of welding wire and filler metal.
Thermal Properties Metric English Comments
Melting Point >= 879.4 °C
>= 1615 °F
Solidus 879.4 °C
1615 °F
Component Elements Properties Metric English Comments
Copper, Cu 52.5 %
52.5 %
Manganese, Mn 38 %
38 %
Nickel, Ni 9.5 %
9.5 %