Valley Adhesives EM-900 High Temperature Application Glue Stick

Category Polymer , Adhesive , Thermoset
Manufacturer Valley Adhesives
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Valley Adhesives EM-900 High Temperature Application Glue Stick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Valley Adhesives EM-900 High Temperature Application Glue StickGeneral purpose; Bonds P.O.P. displays, porous and non-porous substrates, paper, corrugated boxes, fabrics, and foams.
Physical Properties Metric English Comments
Viscosity 6616 cP
6616 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
Tensile Strength, Ultimate 2.76 MPa
400 psi
Elongation at Break 760 %
760 %
Shear Strength 3.13 MPa
454 psi
Peel Strength 4.33 kN/m
24.7 pli
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Heat Resistance Value at 2 psi.
Softening Point 178 °C
352 °F
Processing Properties Metric English Comments
Cure Time 0.133 min
0.00222 hour
Hot tack
Pot Life 0.67 min
0.67 min
Open Time
Descriptive Properties Value Comments
Color Clear