Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Vicone High Performance Rubber VicoFluor™ 57FK-GR High Performance Fluoroelastomer Rubber

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Vicone High Performance Rubber
Trade Name VicoFluor™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Vicone High Performance Rubber VicoFluor™ 57FK-GR High Performance Fluoroelastomer Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Meets ASTM D2000 fluoroelastomer 75 Durometer.
Physical Properties Metric English Comments
Density 2.11 g/cc
0.0762 lb/in³
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
ASTM D2240
Tensile Strength 14.0 MPa
2030 psi
ASTM D412
Elongation at Break 287 %
287 %
ASTM D412
Compressive Modulus 0.0109 GPa

@Strain 5 %
1.58 ksi

@Strain 5 %
ISO-7743
0.0117 GPa

@Strain 10 %
1.70 ksi

@Strain 10 %
ISO-7743
0.0132 GPa

@Strain 20 %
1.91 ksi

@Strain 20 %
ISO-7743
0.0153 GPa

@Strain 25 %
2.22 ksi

@Strain 25 %
ISO-7743
Compression Set 22 %

@Temperature 200 °C,
Time 79200 sec
22 %

@Temperature 392 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature <= -25.0 °C
<= -13.0 °F
passes at 3 min.; ASTM D2137
Descriptive Properties Value Comments
Color Green
Effect of Liquids - Change in Elongation (%) -20
ASTM D471
Effect of Liquids - Change in Hardness (%) -3
ASTM D471
Effect of Liquids - Change in Tensile Strength (%) -23.4
ASTM D471; 23°C; 70 h
Effect of Liquids - Change in Volume after Oil Immersion (%) 4.2
ASTM D471
Heat Aging - Change in Elongation (%) -9.3
ASTM D573; 275°C; 70h
Heat Aging - Change in Hardness (%) 3.5
ASTM D573; 275°C; 70h
Heat Aging - Change in Tensile Strength (%) -1.5
ASTM D573; 275°C; 70h
Users viewing this material also viewed the following: