Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Vicone High Performance Rubber VicoSil™ 369DLK-GY High Performance Silicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Vicone High Performance Rubber
Trade Name VicoSil™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Vicone High Performance Rubber VicoSil™ 369DLK-GY High Performance Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UL94 approved
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
ASTM D2240
Tensile Strength 8.20 MPa
1190 psi
ASTM D412
Elongation at Break 310 %
310 %
ASTM D412
Compressive Modulus 0.00450 GPa

@Strain 5 %
0.653 ksi

@Strain 5 %
ISO-7743
0.00470 GPa

@Strain 10 %
0.682 ksi

@Strain 10 %
ISO-7743
0.00500 GPa

@Strain 20 %
0.725 ksi

@Strain 20 %
ISO-7743
0.00590 GPa

@Strain 25 %
0.856 ksi

@Strain 25 %
ISO-7743
Compression Set 20 %
20 %
ASTM D395
Tensile Set 5.5 %
5.5 %
ASTM D412
Descriptive Properties Value Comments
Color Grey
Effect of Liquids - Change in Elongation (%) -6.1
ASTM D471
Effect of Liquids - Change in Hardness (%) -7
ASTM D471
Effect of Liquids - Change in Tensile Strength (%) -5.7
ASTM D471
Effect of Liquids - Change in Volume after Oil Immersion (%) 6.5
ASTM D471
Heat Aging - Change in Elongation (%) -31.23
ASTM D573
Heat Aging - Change in Hardness (%) 7
ASTM D573; 200°C; 72h
Heat Aging - Change in Tensile Strength (%) -19.88
ASTM D573
Users viewing this material also viewed the following: