Vicone High Performance Rubber VicoSil™ C306E-GR High Performance Silicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Vicone High Performance Rubber
Trade Name VicoSil™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Vicone High Performance Rubber VicoSil™ C306E-GR High Performance Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Vicone
Physical Properties Metric English Comments
Density 1.273 g/cc
0.04599 lb/in³
ASTM D3165
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D2240
53.76

@Treatment Temp. 125 °C,
Time 252000 sec
53.76

@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Tensile Strength, Yield 13.9 MPa
2020 psi
ASTM D412
8.40 MPa

@Treatment Temp. 125 °C,
Time 252000 sec
1220 psi

@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Elongation at Break 602 %
602 %
ASTM D412
375.65 %

@Treatment Temp. 125 °C,
Time 252000 sec
375.65 %

@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Compressive Modulus 0.000710 GPa

@Strain 5.00 %
0.103 ksi

@Strain 5.00 %
0.00126 GPa

@Strain 10.0 %
0.183 ksi

@Strain 10.0 %
0.00183 GPa

@Strain 20.0 %
0.265 ksi

@Strain 20.0 %
0.00238 GPa

@Strain 25.0 %
0.345 ksi

@Strain 25.0 %
Compression Set 6.5 %

@Temperature 100 °C,
Time 252000 sec
6.5 %

@Temperature 212 °F,
Time 70.0 hour
ASTM D395
Descriptive Properties Value Comments
Color Green