Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 8.41 MPa | 1220 psi | ASTM D412 |
Polymax® Maxelast® A9850 TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Strength, Yield | 8.41 MPa | 1220 psi | ASTM D412 |
Polymax® Maxelast® P1885 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 8.40 MPa | 1220 psi | -20% change after 168 hours @ 125°C; ASTM D412 |
Precision Polymer Engineering E60E Ethylene Propylene Rubber Ethylene Propylene Terpolymer, 56-65 °IRHD. Terpolymer of ethylene, propylene and diene monomers. To meet Aerospace Specification DTD5597A Grade 60.Applications: For sealing applications where goo.. |
|||
Tensile Strength, Yield | 8.40 MPa | 1220 psi | 5% change after 70 hours @ 200°C; ASTM D412 |
Precision Polymer Engineering F70A Fluorosilicone Rubber Blue Fluorosilicone Rubber, 60 to 70 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification Mil-R-25988B, Class 1, .. |
|||
Tensile Strength, Yield | 8.40 - 15.6 MPa | 1220 - 2260 psi | ±30% change after 72 hours @ 250°C; ASTM D412 |
Precision Polymer Engineering V70H Fluoroelastomer Compound Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Federal Food and Drug Administ.. |
|||
Tensile Strength, Yield | 8.41 MPa | 1220 psi | ASTM D412 |
Teknor Apex APEX® 3200-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Tensile Strength, Yield | 8.41 MPa | 1220 psi | 100%; ASTM D412 |
Teknor Apex Flexalloy® 3500-75 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te.. |
|||
Tensile Strength, Yield | 8.41 MPa | 1220 psi | ASTM D412 |
Teknor Apex APEX® 3300-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Food Service Applications, General Purpose, Me.. |
|||
Tensile Strength, Yield | 8.40 MPa @Treatment Temp. 125 °C, Time 252000 sec |
1220 psi @Treatment Temp. 257 °F, Time 70.0 hour |
Heat Aging; ASTM D573 |
Vicone High Performance Rubber VicoSil™ C306E-GR High Performance Silicone Rubber Information provided by Vicone |
|||
Tensile Strength, Yield | 8.41 MPa | 1220 psi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 2890 Thermoplastic Elastomer Elastocon® 2890 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2890 is FDA compliant and well suited for cons.. |