Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Victrex® Vicote® F807 Black Polyetheretherketone (PEEK) Liquid Dispersion

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Victrex
Trade Name Vicote®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Victrex® Vicote® F807 Black Polyetheretherketone (PEEK) Liquid Dispersion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eco-friendly VICOTE Coatings were developed to fill the performance gap found in many existing coating technologies today. Whether applied to industrial, automotive, food processing, semiconductor, electronics or pharmaceutical parts. VICOTE Coatings can be applied using electrostatic or conventional dispersion spray techniques.The main ingredient of VICOTE Coatings is VICTREX® PEEK polymer, a linear, aromatic, semi-crystalline thermoplastic, widely regarded as one of the highest performing thermoplastic materials in the world. It offers a unique combination of properties to help processors and end users reach new levels of cost savings, performance, and product differentiation.These grades have been specifically formulated to provide a tough, resilient, high wear resistant coating with varying levels of lubricants to give good release properties. Available in natural and black. Electrostatic dissipative (ESD) grade. All other grades are Insulative coatings.F-Grades of VICOTE Coatings are specially formulated by Victrex to solve the problem of flash rusting that can occur when water-based coatings are applied to ferrous metals such as mild steel. Can also coat non-ferrous substrates equally effectively.All information provided by Victrex.
Physical Properties Metric English Comments
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Impact 1.0
1.0
1m, 1kg, Indent 5mm; ISO 6272
Coefficient of Friction 0.165
0.165
µm @ 10 min., Using 250N Load; ASTM G 133
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Processing Properties Metric English Comments
Drying Temperature 120 °C
248 °F
overnight before use
150 °C

@Time 10800 sec
302 °F

@Time 3.00 hour
Descriptive Properties Value Comments
Color Black
Konig Hardness (seconds) 140
ISO 1522